     Inclusions 
 
Usually caused by Cured by
Improper sprues. Eliminate sharp corners in sprue system.
Crucible break down Replace crucible. Do not used old, disintegrating crucibles.
Dirty metal Do not use more than 50% recycled alloy and ensure it is clean.
Flasks overheated during burnout. Ensure maximum burnout temperature does not exceed 740ºC.
 
  Casting problems
  Wax pattern problems
  Mould rubber problems
Mixing guide